I've been noticing some delamination (layer separation), but only on solid infill and top layers, and only on larger surfaces

Initially, I tried reducing speed, but didn't notice any improvement

There are no noticeable issues on short lines, so I think this is something to do with acceleration, which I didn't realise was a thing, but there are indeed settings for this in OrcaSlicer

Update:

Reducing acceleration does seem to have resulted in less severe delamination, but it hasn't gone away completely

So I think I need to reduce it just a little bit more

you are viewing a single comment's thread
view the rest of the comments
[-] jokeyrhyme@lemmy.ml 1 points 1 week ago

for this 230C - 250C PETG filament, i'm already at 250C (but i've been contemplating bumping it up to 255C)

this post was submitted on 27 Sep 2025
2 points (100.0% liked)

3DPrinting

19920 readers
61 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS