When I do an overhang test, I always have this problem at about 35°. Does anyone have a suggestion what could be causing it?

  • Slicer: Orca
  • Layer height: 0.2mm
  • Infill: 0% (this has improved it a lot, I think the infill was causing bulging)
  • Outer walls: 2
  • Overhang speed: 10 or 20mm/s (both look the same)

Solution: I mistakenly thought overhang speed in Orca was based on overhang angle, it is percentage instead (which makes much more sense for different layer heights). My 10-25% overhang speed wasn't set to slow down and that must translate to about 35° at 0.2mm layer height. I now have it set to 30mm/s and it now looks great 👍 And sorry, I was wrong when I stated the overhang speed 😅

you are viewing a single comment's thread
view the rest of the comments
[-] UnH1ng3d@lemmy.world 3 points 7 months ago

Thanks. I'll experiment with temperatures first but I've got some different filament on the way too as it happens, so hopefully I'll manage to escape the problem one way or another 😁

this post was submitted on 12 Apr 2024
43 points (97.8% liked)

3DPrinting

15548 readers
100 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS