I've been noticing some delamination (layer separation), but only on solid infill and top layers, and only on larger surfaces

Initially, I tried reducing speed, but didn't notice any improvement

There are no noticeable issues on short lines, so I think this is something to do with acceleration, which I didn't realise was a thing, but there are indeed settings for this in OrcaSlicer

Update:

Reducing acceleration does seem to have resulted in less severe delamination, but it hasn't gone away completely

So I think I need to reduce it just a little bit more

you are viewing a single comment's thread
view the rest of the comments
[-] teotwaki@lemmy.world 2 points 1 week ago

I've been seeing your posts on Masto, but I guess I'll reply here.

I don't know what printer you have, and I don't know if the feature works for all printers, but could you try and use PrusaSlicer to visualise the print where the issue presents itself. More specifically, you could get some interesting data from the "actual print speed" view. That way you can see what speed the printhead reaches.

However, based on your description:

  • when the printer reaches high print speeds you get delam
  • slowing down the print head reduces (but doesn't eliminate delam)

Could you be reaching the limit of what your printhead can melt? Would it make sense to calculate the actual flow through your nozzle at those high speeds? Finally, how much part cooling do you have setup? Have you tried a skirt to keep the temps more consistent?

[-] jokeyrhyme@lemmy.ml 2 points 1 week ago* (last edited 1 week ago)

okay, just viewing the job layer by layer, i can see that the first solid infill layer after the sparse infill is treated as an overhang/bridge and triggers 100% cooling fan (otherwise it's at 0% for the rest of the print)

and on some items, i can see where the delamination on this layer caused problems on the next couple of layers on top

but, on other items, there's still delamination happening on the very top layer even without any issues beneath it

[-] jokeyrhyme@lemmy.ml 1 points 1 week ago
  • Sovol3D SV06 ACE
  • OrcaSlicer recently gained a built-in profile for exactly this model, and I've had all sorts of issues since switching to that profile (previously I started with a generic printer profile)
  • the new profile is fine on PLA, but PETG is what I'm currently using
  • yeah, I only just learnt about the print visualisation feature, the delamination does seem to frequent the same place on the object/plate
  • it's the 6x6 panel from https://www.printables.com/model/859807-print6-panels
  • the spans from cross hole to cross hole are short and never delaminate
  • the long straight edge-to-edge spans that dodge the holes have been troublesome
  • the plan is to reduce acceleration a bit more, and then (if that doesn't help) reduce speed a bit (I've already reduced speed and filament volume anyway because of PETG)
this post was submitted on 27 Sep 2025
2 points (100.0% liked)

3DPrinting

19920 readers
61 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS