Hi there,

I’m wondering if I could get some advice on why my prints are always failing at 0.2mm layer height

Attached is a pic, the first layers are perfect but as it gets to layer 3-4 I the print does not stick to the previous layers!

Printing at 0.1mm is absolutely perfect, first layer is perfect etc (in my opinion)

Just wanted to have the option for a 0.2mm height so the prints don’t take as long.

Printer is Kingroon KP3S Pro V2 with Klipper Slicer is OrcaSlicer

I can share configs from either if needed, or more close up pics.

Cheers

you are viewing a single comment's thread
view the rest of the comments
[-] Rutty@sh.itjust.works 3 points 1 year ago

Would bumping up your printing temp do anything?

[-] nath@lemm.ee 2 points 1 year ago

It's already running 225 for PLA since it's a hardened steel nozzle, but I tried it on 230 with the same result

this post was submitted on 19 Sep 2023
12 points (100.0% liked)

3DPrinting

15599 readers
61 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS