49

Printing here with eSun PLA at 215 C on a Prusa Mini, and there are lots of hairline strings.

What's causing those strings? Temp too low?

you are viewing a single comment's thread
view the rest of the comments
[-] kilted_cyclist@lemmy.world 1 points 11 months ago

I can't add anything concerning stringing that the other comment didn't already cover, so I'll ask about the gaps.

Have you tried upping the flow rate to fill them in? The other option I've used in the past was lowering my Z Offset if the flow was alright.

Keep in mind that changing your flow rate will likely also cause you have to mess with your retraction settings again.

this post was submitted on 16 Nov 2023
49 points (98.0% liked)

3DPrinting

15493 readers
192 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS