55

Got an anycubic resin printer and I'm using their high speed resin (because it was bundled for free), and i tried to send a file using the high speed setting.

After the print it was seemed to be ok, then after i left in a bath of ethanol (IPA can't be found in stores in my country) i got all those holes.

What's the problem?

A slicer problem? The ethanol bath? The high speed resin that's not good?

you are viewing a single comment's thread
view the rest of the comments
[-] plandeka@lemmy.world 8 points 7 months ago* (last edited 7 months ago)

They look like air bubbles to me, but it is weird they only come out after the bath. Could be they were already inside, but only covered by a thin wall of resin.

I usually use Isopropanol for bath not Ethanol, so I am not sure how your resin reacts with that. The bath should also be rather short, like 1min or something.

A few things to try:

  • If you are shaking your resin before print, then give it like 10 minutes after you pour it into the vat, so all bubbles come out and pop
  • lower the print speed
  • add wait times between the end of lowering the plate and light on
  • try to hollow out the model if possible, so there is less printing volume
this post was submitted on 26 Mar 2024
55 points (98.2% liked)

3DPrinting

15606 readers
121 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS